SM-42

Copper & Copper Alloys (TIG/MIG)

Alloy Basis:

Phosphor Bronze (CuSn8P)

DETAILS

Copper & Copper Alloys (TIG/MIG)

Applications

Senor Phosphor Bronze C filler metal is used quite extensively for surfacing applications. The higher tin content, gives Phosphor-Bronze C weld deposits greater hardness and higher tensile/yield strength than C51800 (Phos-Bronze A). It is used for joining brass and bronze alloys and joining cast Iron to carbon steel.

Disclaimers

Service Information

Documentation

  • Safety Data Sheet
  • Certificates of Conformance

More Products

CHEMICAL COMPOSITIONS

Cu Fe Ni P Pb Sn Zn Others
bal. 0.1 0.2 0.1 to 0.4 0.02 7.5 to 8.5 0.2 0.2

 

PHYSICAL AND MECHANICAL PROPERTIES

Solidus Temperature 875°C (1607°F) Liquidus Temperature 1025°C (1877°F)
Density 8.8 gms/cm3 Tensile Strength 260 N/mm2
Elongation 20% Brinell Hardness 80HB